X46Cr13   ( 1.4034 )

    Grade :     X46Cr13
    Number:     1.4034
    Classification:     Martensitic stainless steel
    Density:     7.7   g/cm ³
    Standard:
    EN 10088-2: 2005 Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
    EN 10088-3: 2005 Stainless steels. Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
    EN 10088-1: 2005 Stainless steels. List of stainless steels
    Equivalent grades:     Go here



Chemical composition %   of grade   X46Cr13 (1.4034):   EN 10088-2-2005
Tighter carbon ranges may be agreed at the time of enquery and order
Particular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted. For weldability, a controlled sulphur content of 0.008 % to 0.030 % is recommended and permitted. For polishability, a controlled sulphur content of 0.015 % max is recommended.
Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast.
C Si Mn P S Cr
0.43 - 0.5max   1max   1max   0.04max   0.01512.5 - 14.5


Mechanical properties of grade   X46Cr13 (1.4034)

Rm - Tensile strength (MPa) (+A)780
Rm - Tensile strength (MPa) (+QT800)850-1000


Rp0.2 0.2% proof strength (MPa) +QT800650


KV - Impact energy (J) longitud., +20°
12


A - Min. elongation at fracture (%) 10-12


  Brinell hardness   (HB):   (+A)245


Equivalent grades of grade   X46Cr13 (1.4034)
Warning! Only for reference

Poland
PN
Russia
GOST
4H13
40KH13


Mechanical properties
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc


Heat treatment conditions

+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

Martensitic stainless steel   X46Cr13 (1.4034)
Chemical composition , Equivalent grades , Standards, Properties , Hardness , Strength , Elongation

European Steel and Alloy Grades / Numbers   ©   2011- 2015   All rights reserved.     The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user