GX5CrNiMoNb19-11-2   ( 1.4581 )

    Grade :     GX5CrNiMoNb19-11-2
    Number:     1.4581
    Classification:     Austenitic corrosion resistant casting steel
    Density:     7.9   g/cm ³
    EN 10213: 2007 Steel castings for pressure purposes
    EN 10283: 2010 Corrosion resistant steel castings
    Equivalent grades:     No information

Chemical composition %   of grade   GX5CrNiMoNb19-11-2 (1.4581):   EN 10213-2007
The niobium content value applies for the sum of the niobium + tantalum.
C Si Mn Ni P S Cr Mo Nb Cu
max   0.07max   1.5max   1.59 - 12max   0.04max   0.0318 - 202 - 2.5max   1max   0.5

Mechanical properties of grade   GX5CrNiMoNb19-11-2 (1.4581)

Rm - Tensile strength (MPa) (+AT)440-640

Rp0.2 0.2% proof strength (MPa) (+AT)185

KV - Impact energy (J) (+AT)+20°

A - Min. elongation at fracture (%) (+AT)25

Mechanical properties
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc

Heat treatment conditions

+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

  GX5CrNiMoNb19-11-2 (1.4581) - Austenitic corrosion resistant casting steel
Chemical composition , Equivalent grades of Steel, Standards, Mechanical Properties, Hardness , Strength , Elongation

European Steel and Alloy Grades / Numbers Searchable Database   ©   2011- 2016   All rights reserved.     About us. Contacts.
The contents from this site may not be reproduced.   The entire risk as to use of these content is assumed by you the user