GP240GH   ( 1.0619 )

    Grade :     GP240GH
    Number:     1.0619
    Standard:
    EN 10213 : 2007   Steel castings for pressure purposes
    Density:     7.8   g/cm ³
    Classification:     Cast steel
    Equivalent grades:     Go here



Chemical composition %   of grade   GP240GH (1.0619)
C Si Mn Ni P S Cr Mo V Cu
0.18 - 0.23max   0.60.5 - 1.2max   0.4max   0.03max   0.02max   0.3max   0.12max   0.03max   0.3


Mechanical properties of grade   GP240GH (1.0619)

Rm - Tensile strength (MPa) (+QT)420-600


Rp0.2 0.2% proof strength (MPa) (+QT)240


KV - Impact energy (J) (+QT)+20°
40
KV - Impact energy (J) (+N)+20°
27


A - Min. elongation at fracture (%) (+QT)22


Equivalent grades of grade   GP240GH (1.0619)
Warning! Only for reference
Germany
DIN,WNr
China
GB
GS-C25N
ZG230-450


Mechanical properties
Mechanische Eigenschaften
Caracteristiques mecaniques
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc


Heat treatment conditions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

Cast steel   GP240GH (1.0619), Chemical composition of   GP240GH (1.0619). Equivalent grades of   GP240GH (1.0619). Standards of   GP240GH (1.0619).
Properties of   GP240GH (1.0619). Hardness of   GP240GH (1.0619). Strength of   GP240GH (1.0619). Elongation of   GP240GH (1.0619).

©   2011- 2014   All rights reserved.       The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user