X15CrNiSi20-12   ( 1.4828 )


    Grade :     X15CrNiSi20-12
    Number:     1.4828
    Classification:     Austenitic heat-resisting steel
    Density:     7.9   g/cm ³
    Standard:
    EN 10095: 1999 Heat Resisting Steels and Nickel Alloys
    EN 10296-2: 2005 Welded circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions
    EN 10088-1: 2005 Stainless steels. List of stainless steels
    Equivalent grades:     Go here



Chemical composition %   of grade   X15CrNiSi20-12 (1.4828):   EN 10095-1999
C Si Mn Ni P S Cr N
max   0.21.5 - 2.5max   211 - 13max   0.045max   0.01519 - 21max   0.11


Mechanical properties of grade   X15CrNiSi20-12 (1.4828)

Rm - Tensile strength (MPa) (+AT)550-750


Rp0.2 0.2% proof strength (MPa) (+AT)230


A - Min. elongation at fracture (%) (+AT)28-30


  Brinell hardness   (HB):   (+AT)223


Properties of grade   X15CrNiSi20-12 (1.4828)
Maximum application temperature for air T= 1000 ° C


Equivalent grades of grade   X15CrNiSi20-12 (1.4828)
Warning! Only for reference
USA
-
Germany
DIN,WNr
Japan
JIS
France
AFNOR
England
BS
Italy
UNI
China
GB
Poland
PN
Czechia
CSN
Russia
GOST
309
X15CrNiSi20-12
SUH309
Z17CNS20-12
309S24
X16CrNi23-14
1Cr20Ni14Si2
H20N12S2
17251
20KH20N14S2


Mechanical properties
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc


Heat treatment conditions

+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

  X15CrNiSi20-12 (1.4828) - Austenitic heat-resisting steel
Chemical composition , Equivalent grades of Steel, Standards, Mechanical Properties, Hardness , Strength , Elongation


European Steel and Alloy Grades / Numbers Searchable Database   ©   2011- 2016   All rights reserved.     About us. Contacts.
The contents from this site may not be reproduced.   The entire risk as to use of these content is assumed by you the user