SteelNumber: European Steel and Alloy Grades / Numbers Database
          Home Steel Numbers Steel and Cast Iron Standards Alloy Standards Search Buy / Sell Product Worldwide Equivalents About Us          
YOU HERE:   Steel Numbers   ->   Number 1.45XX           OR           Steel & Cast Iron Standards   ->     /   EN 10088-2   /   EN 10088-3   /   EN 10028-7   /   EN 10216-5   /   EN 10253-3   /   EN 10253-4   /   EN 10272   /   EN 10250-4   /   EN 10297-2   /   EN 10088-1

X2CrNiMoCuN25-6-3   ( 1.4507 )


    Grade :     X2CrNiMoCuN25-6-3
    Number:     1.4507
    Classification:     Austenitic-ferritic stainless steel - special grade
    Density:     7.8   g/cm ³
    Standard:
    EN 10088-2: 2005 Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
    EN 10088-3: 2005 Stainless steels. Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
    EN 10028-7: 2007 Flat products made of steels for pressure purposes. Stainless steels
    EN 10216-5: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Stainless steel tubes
    EN 10253-3: 2008 Butt-welding pipe fittings. Wrought austenitic and austenitic-ferritic (duplex) stainless steels without specific inspection requirements
    EN 10253-4: 2008 Butt-welding pipe fittings. Wrought austenitic and austenitic-ferritic (duplex) stainless steels with specific inspection requirements
    EN 10272: 2007 Stainless steel bars for pressure purposes
    EN 10250-4: 2000 Open steel die forgings for general engineering purposes. Stainless steels
    EN 10297-2: 2005 Seamless circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions
    EN 10088-1: 2005 Stainless steels. List of stainless steels
    Equivalent grades:     No information



Chemical composition %   of   steel   X2CrNiMoCuN25-6-3 (1.4507):   EN 10088-2-2005
Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast.
C Si Mn Ni P S Cr Mo N Cu
max   0.03max   0.7max   26 - 8max   0.035max   0.01524 - 263 - 40.2 - 0.31 - 2.5


Mechanical properties of   steel   X2CrNiMoCuN25-6-3 (1.4507)

Rm - Tensile strength (MPa) (+A)690-1000
Rm - Tensile strength (MPa) (+AT)700-900


Rp0.2 0.2% proof strength (MPa) (+A)500-550
Rp0.2 0.2% proof strength (MPa) (+AT)500


KV - Impact energy (J) transverse, (+A)+20°
90
-40°
40
KV - Impact energy (J) longitud., (+A)+20°
100-150
KV - Impact energy (J) longitud., (+AT)+20°
100
KV - Impact energy (J) transverse, (+AT)+20°
100
-40°
40


A - Min. elongation at fracture (%) (+A)20-25
A - Min. elongation at fracture (%) longitud., (+AT)20


  Brinell hardness   (HB):   (+A)270
  Brinell hardness   (HB):   (+AT)310


Properties of   steel   X2CrNiMoCuN25-6-3 (1.4507)
Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes

NEW opportunities for buyers!
Post free buying requirement   of   steel   X2CrNiMoCuN25-6-3 (1.4507)



Mechanical properties
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc


Heat treatment conditions

+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

Austenitic-ferritic stainless steel - special grade
Chemical composition of   steel   X2CrNiMoCuN25-6-3 (1.4507), Standards of   steel   X2CrNiMoCuN25-6-3 (1.4507)
Mechanical Properties of   steel   X2CrNiMoCuN25-6-3 (1.4507)
Tensile Strength, Elongation, Proof strength, Hardness


European Steel and Alloy Grades / Numbers Searchable Database   ©   2011- 2018   All rights reserved.     About us. Contacts.
The contents from this Steel & Alloy Database may not be reproduced.   The entire risk as to use of these content is assumed by you the user
Google+   SteelNumber