EUROPEAN STEEL AND ALLOY GRADES |
| Home | Steel numbers | Steel and cast iron standards | Alloy standards | Equivalent grades | Search | Russian steels | About us |
| YOU HERE: Alloy standards -> Brazing, soldering, welding - all grades OR Alloy standards -> / EN 14172 |
| Grade : | NiCr22Mo7Fe19 |
| Number: | Ni6985 |
| Standard: | EN ISO 14172 : 2008 Welding consumables. Covered electrodes for manual metal arc welding of nickel and nickel alloys. Classification |
| Classification: | Nickel-chromium-molybdenum alloy |
| Equivalent grades: | Go here |
| Up to 1% of the nickel content can be cobalt Up to 20% of the niobium content can be tantalum The total of unspecified elements shall not exceed 0.5% excluding cobalt and tantalum |
| Fe | C | Si | Mn | Ni | P | S | Cr | Mo | W | Co | Nb | Cu |
| 18 - 21 | max 0.02 | max 1 | max 1 | min 45 | max 0.02 | max 0.015 | 21 - 23.5 | 6 - 8 | max 1.5 | max 5 | max 1 | 1.5 - 2.5 |
| Rm - Tensile strength (MPa) | 620 |
| Rp0.2 0.2% proof strength (MPa) | 350 |
| A - Min. elongation at fracture (%) (5d) | 22 |
| USA - | Germany DIN,WNr | ||
|
|
| ReH | Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale |
| Rm | Tensile strength / Zugfestigkeit / Resistance a la traction |
| A | Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal |
| J | Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc |
| The entire risk as to use of these content is assumed by you the user |