  CuZn37   ( CW508L )

    Grade :     CuZn37
    Number:     CW508L
    Classification:     Copper-zinc alloy
    Density     8.4 g/cm ³
    Standard: EN 1652: 1998 Copper and copper alloys. Plate, sheet, strip and circles for general purposes
EN 12163: 1998 Copper and copper alloys. Rod for general purposes
EN 12166: 1998 Copper and copper alloys. Wire for general purposes
EN 12167: 1998 Copper and copper alloys. Profiles and rectangular bar for general purposes
EN 12165: 1998 Copper and copper alloys. Wrought and unwrought forging stock
EN 12449: 1999 Copper and copper alloys. Seamless, round tubes for general purposes
EN 12420: 1999 Copper and copper alloys. Forgings
EN 13148: 2001 Copper and copper alloys. Hot-dip tinned strip
    Equivalent grades:     Go here



Chemical composition %   of grade   CuZn37   ( CW508L )
Fe NiAl Cu PbSn Others -
max   0.1max   0.3max   0.0562 - 64max   0.1max   0.1 total 0.1 Zn - remainder


Mechanical properties of grade   CuZn37   ( CW508L )

Rm - Tensile strength (MPa) (R300)300-370
Rm - Tensile strength (MPa) (R350)350-440
Rm - Tensile strength (MPa) (R410)410-490


Rp0.2 0.2% proof strength (MPa) (R300)180
Rp0.2 0.2% proof strength (MPa) (R350)170
Rp0.2 0.2% proof strength (MPa) (R410)300


A - Min. elongation at fracture (%) (R300)48
A - Min. elongation at fracture (%) (R350)28
A - Min. elongation at fracture (%) (R410)12


A - Min. elongation Lo = 50mm (%) (R300) 38
A - Min. elongation Lo = 50mm (%) (R350) 19
A - Min. elongation Lo = 50mm (%) (R410) 8


  Vickers hardness  ( HV):   (H055)55 - 95
  Vickers hardness  ( HV):   (H095)95 - 125
  Vickers hardness  ( HV):   (H120)120 - 155


Equivalent grades of grade   CuZn37   ( CW508L )
Warning! Only for reference
Germany
DIN,WNr
2.0321
CuZn37


Casting process
GS Sand casting
GM Permanent mould casting
GZ Centrifugal casting
GC Continuous casting
GP Pressure die casting


Material conditions
R Material condition designated by the minimum value of tensile strength requirement for the product with mandatory tensile strength and elongation requirements
H Material condition designated by the minimum value of hardness requirement for the product with mandatory hardness requirements


Mechanical properties
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d´┐Żelasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc

Copper-zinc alloy   CuZn37   ( CW508L )
Chemical composition of   CuZn37   ( CW508L ). Equivalent grades of   CuZn37   ( CW508L ).
Standards of   CuZn37   ( CW508L ). Properties of   CuZn37   ( CW508L ). Hardness of   CuZn37   ( CW508L ).

European Steel and Alloy Grades / Numbers   ©   2011- 2015   All rights reserved.     The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user