  ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 )

    Grade :     ENAC-AlSi9Cu3(Fe)
    Number:     ENAC-46000
    Standard: EN 1706 : 2010   Aluminium and aluminium alloys. Castings. Chemical composition and mechanical properties
    Classification:     Aluminium alloy for casting
    Equivalent grades:     Go here


Chemical composition %   of grade   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 )
Fe Si Mn Ni Cr Ti Cu Pb Mg Zn Sn Others -
max   1.38 - 11max   0.55max   0.55max   0.15max   0.252 - 4max   0.350.05 - 0.55max   1.2max   0.15each 0.05; total 0.25 Al - remainder


Mechanical properties of grade   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 )

Rm - Tensile strength (MPa) (F) (D)240


Rp0.2 0.2% proof strength (MPa) (F) (D)140


A - Min. elongation at fracture (%) (F) (D)1


  Brinell hardness   (HBW):   (F) (D)80


Equivalent grades of grade   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 )
These comparison tables are only intended as an indication of the closest khown equivalent grades.
Germany
DIN,WNr
Japan
JIS
Inter
ISO
3.2163
GD-AlSi9Cu3
ADC10
AlSi9Cu3(Fe)


Temper designations
O Annealed
H Strain hardened
F Fabricated (as cast)
T Thermally treated to produce stable tempers other than F, O or H
T1 Cooled from an elevated temperature shaping process and naturally aged
T2 Cooled from an elevated temperature shaping process, cold worked and naturally aged
T3 Solution heat treated, cold worked and naturally aged
T4 Solution heat treated and naturally aged
T5 Cooled from an elevated temperature shaping process and then artificially aged
T6 Solution heat treated and then artificially aged
T7 Solution heat treated and then artificially overaged (stabilised)
T8 Solution heat treated, cold worked and then artificially aged
T9 Solution heat treated, artificially aged and then cold worked
W Solution heat treated (unstable temper)
EN 515:1993 Aluminium and aluminium alloys. Wrought products. Temper designations


Casting processes
S Sand casting
K Chill or permanent mould casting
D Pressure die casting
L Investment casting

Chemical composition of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Equivalent grades of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Standards of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ).
Properties of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Hardness of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Strength of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Elongation of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ).


Mechanical properties
Mechanische Eigenschaften
Caracteristiques mecaniques
ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc

Chemical composition of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Equivalent grades of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ).
Standards of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Properties of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ). Hardness of   ENAC-AlSi9Cu3(Fe)   ( ENAC-46000 ).

©   2011- 2014   All rights reserved.       The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user